简体中文

ZYH1-1-A

Performance
Casting Mode Tensile Strength
Rm(MPa)
Yield Strength
Rp0.2(MPa)
Elongation
A(%)
Brinell Hardness
(HBW)
Conductivity
(%IACS)
Thermal Conductivity
W/(m·K)
Heat Treatment Mold Characteristic
Recasting               T6 High Hardness
Main Components
Si Fe Cu  Mn  Mg Zn Ti Cr Pb Al