ADC10-1-A

Performance
Casting Mode Tensile Strength
Rm(MPa)
Yield Strength
Rp0.2(MPa)
Elongation
A(%)
Brinell Hardness
(HBW)
Conductivity
(%IACS)
Thermal Conductivity
W/(m·K)
Heat Treatment Mold Characteristic
Die-casting ≥241 ≥157 ≥1.5 ≥73.6       F High Tensile
Main Components
Si Fe Cu  Mn  Mg Zn Ti Cr Ni Pb Sn Cd Al
7.5~9.5 0.6-1.0 2.0~4.0 ≤0.50 ≤0.30 ≤1.0 ≤0.3 ≤0.10 ≤0.50 <0.10 ≤0.20 <0.01 Tolerance