ADC6-3-A

Performance
Casting Mode Tensile Strength
Rm(MPa)
Yield Strength
Rp0.2(MPa)
Elongation
A(%)
Brinell Hardness
(HBW)
Conductivity
(%IACS)
Thermal Conductivity
W/(m·K)
Heat Treatment Mold Characteristic
Die-casting ≥266 ≥172 ≥6.4 ≥64.7       F Anti-corrosion/Super Toughness
Main Components
Si Fe Cu  Mn  Mg Zn Ni Sn Al
≤1.0 ≤0.6 ≤0.10 0.4~0.6 2.6~4.0 ≤0.40 ≤0.10 ≤0.10 Tolerance