771-6-A

Performance
Casting Mode Tensile Strength
Rm(MPa)
Yield Strength
Rp0.2(MPa)
Elongation
A(%)
Brinell Hardness
(HBW)
Conductivity
(%IACS)
Thermal Conductivity
W/(m·K)
Heat Treatment Mold Characteristic
Recasting               T6 High Tensile/High Hardness
Main Components
Si Fe Cu  Mn  Mg Zn Ti Cr Al
≤0.15 ≤0.12 ≤0.10 ≤0.10 0.9~1.1 6.5~7.5 0.1~0.2 0.06~0.20 Tolerance