| Casting Mode | Tensile Strength Rm(MPa) |
Yield Strength Rp0.2(MPa) |
Elongation A(%) |
Brinell Hardness (HBW) |
Conductivity (%IACS) |
Thermal Conductivity W/(m·K) |
Heat Treatment Mold | Characteristic | |
| Recasting | T6 | High Tensile/High Hardness | |||||||
| Si | Fe | Cu | Mn | Mg | Zn | Ti | Cr | Other | Al | |
| ≤0.15 | ≤0.40 | ≤0.25 | ≤0.10 | 0.65~0.70 | 6.5~7.3 | 0.15~0.25 | 0.40~0.60 | Mg is an exceptional case (fire waste) | Tolerance | |