- 简体中文
 

| Casting Mode | Tensile Strength Rm(MPa)  | 
			Yield Strength Rp0.2(MPa)  | 
			Elongation A(%)  | 
			Brinell Hardness (HBW)  | 
			Conductivity (%IACS)  | 
			Thermal Conductivity W/(m·K)  | 
			Heat Treatment Mold | Characteristic | |
| Recasting | T6 | High Tensile | |||||||
| Si | Fe | Cu | Mn | Mg | Zn | Ti | Cr | Ni | Pb | Cd | Hg | Other | Al | 
| 5.0~7.0 | <1.0 | 3.5~5.0 | 0.4~0.6 | 0.1~0.3 | <2.0 | <0.2 | <0.1 | <0.3 | <0.1 | <0.01 | <0.1 | Except SI,AI,CU,Impurity All<2.0 | Tolerance |