简体中文

AlSi10MnMg-2-D

Performance
Casting Mode Tensile Strength
Rm(MPa)
Yield Strength
Rp0.2(MPa)
Elongation
A(%)
Brinell Hardness
(HBW)
Conductivity
(%IACS)
Thermal Conductivity
W/(m·K)
Heat Treatment Mold Characteristic
Die-casting              Heat Treatment T4/T5/T6/T6 Super Toughness
Main Components
Si Fe Cu  Mn  Mg Zn Ti Other Al
9.0-11.5 ≤0.20 ≤0.03 0.4-0.8 0.15-0.60 ≤0.07 ≤0.15 Only≤0.05  all≤0.15 Tolerance