简体中文

A356.2-1-A

Performance
Casting Mode Tensile Strength
Rm(MPa)
Yield Strength
Rp0.2(MPa)
Elongation
A(%)
Brinell Hardness
(HBW)
Conductivity
(%IACS)
Thermal Conductivity
W/(m·K)
Heat Treatment Mold Characteristic
Die-casting/Semisolid/Squeeze Casting/Recasting               T6 Super Toughness
Main Components
Si Fe Cu  Mn  Mg Zn Ti Pb Cd Other Al
6.5~7.5 ≤0.12 ≤0.1 ≤0.05 0.30~0.45 ≤0.05 ≤0.20 ≤0.05 ≤0.01 Only≤0.05    all≤0.15 91.3-93.2