6063-1-A

Performance
Casting Mode Tensile Strength
Rm(MPa)
Yield Strength
Rp0.2(MPa)
Elongation
A(%)
Brinell Hardness
(HBW)
Conductivity
(%IACS)
Thermal Conductivity
W/(m·K)
Heat Treatment Mold Characteristic
Squeeze Casting               T6 Anti-corrosion
Main Components
Si Fe Cu  Mn  Mg Zn Ti Cr Ni Pb Sn Al
0.20~0.60 ≤0.35 ≤0.10 ≤0.10 0.45~0.90 ≤0.10 ≤0.10 ≤0.10 ≤0.05 ≤0.05 ≤0.05 Tolerance