简体中文

356.1-1-A

Performance
Casting Mode Tensile Strength
Rm(MPa)
Yield Strength
Rp0.2(MPa)
Elongation
A(%)
Brinell Hardness
(HBW)
Conductivity
(%IACS)
Thermal Conductivity
W/(m·K)
Heat Treatment Mold Characteristic
Die-casting/Semisolid/Squeeze Casting               T6 Super Toughness
Main Components
Si Fe Cu  Mn  Mg Zn Ti Al
6.5-7.5 ≤0.6 ≤0.25 ≤0.35 0.25~0.45 ≤0.35 ≤0.25 Tolerance